Because it cycles at 75oC, polyvinyl chloride vessels are sufficient to replace the expensive metal vessels that are normally required. To make the material, waste plastic is turned into powder, mixed with potassium acetate and heated at 600oC for 45 minutes to optimise the pores, most of which are about 0.7nm wide. …Read the full […]